Solvay TECHNYLSTARâ„¢ S 216L2 V30 PA6, 30% glass filled, DRY

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 30% Glass Fiber Filled
Manufacturer Solvay
Trade Name TECHNYLSTAR™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay TECHNYLSTARâ„¢ S 216L2 V30 PA6, 30% glass filled, DRY.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: TECHNYLSTAR polyamide reinforced with 30% GF, UV stabilized, for Injection molding. Available in: Europe and North AmericaProduct Applications: TECHNYLSTAR TM S 216L2 V30 BLACK is characterized by general good mechanical properties and high impact resistance in external environment. It is particularly suitable for automotive external parts requiring UV resistance, like door handles, windshield frames, etc. This product is available in black.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Mechanical Properties Metric English Comments
Tensile Strength at Break 160 MPa
23200 psi
ISO 527 Type 1A
Elongation at Break 2.1 %
2.1 %
ISO 527 Type 1A
Tensile Modulus 10.4 GPa
1510 ksi
ISO 527 Type 1A
Charpy Impact Unnotched 4.50 J/cm²
21.4 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 0.810 J/cm²
3.85 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 222 °C
432 °F
ISO 11357
Processing Properties Metric English Comments
Feed Temperature 220 - 225 °C
428 - 437 °F
Front Barrel Temperature 240 - 245 °C
464 - 473 °F
Mold Temperature 80.0 °C
176 °F
Drying Temperature 80.0 °C
176 °F
Moisture Content <= 0.15 %
<= 0.15 %
Descriptive Properties Value Comments
Compression Zone 235-240°C