Solvay TECHNYLSTARâ„¢ S 218 MT PA6, 40% mineral filled, Conditioned

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 40% Mineral Filled
Manufacturer Solvay
Trade Name TECHNYLSTAR™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay TECHNYLSTARâ„¢ S 218 MT PA6, 40% mineral filled, Conditioned.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: TechnylStar Polyamide, 40% mineral filled, heat stabilized, for injection molding. Characterized by a high fluidity of the melt.Available in: Asia Pacific and North AmericaProduct Applications: This grade has good mechanical properties. It is suitable for automotive industry and specially designed for electroplating. This product is available in naturalInformation provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.45 g/cc
0.0524 lb/in³
ISO 1183/A
Mechanical Properties Metric English Comments
Tensile Strength at Break 55.0 MPa
7980 psi
ISO 527 Type 1A
Elongation at Break 25 %
25 %
ISO 527 Type 1A
Tensile Modulus 2.60 GPa
377 ksi
ISO 527 Type 1A
Flexural Strength 65.0 MPa
9430 psi
ISO 178
Flexural Modulus 1.85 GPa
268 ksi
ISO 178
Izod Impact, Notched (ISO) 7.00 kJ/m²
3.33 ft-lb/in²
ISO 180/1eA
Izod Impact, Unnotched (ISO) 150 kJ/m²
71.4 ft-lb/in²
ISO 180/1eU
Charpy Impact Unnotched 22.0 J/cm²
105 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 0.650 J/cm²
3.09 ft-lb/in²
ISO 179/1eA
Processing Properties Metric English Comments
Moisture Content <= 0.20 %
<= 0.20 %