Material Notes:
Polyamide PA6, reinforced with 30% of glass fiber, for injection molding.It has good mechanical properties. It is used in all sectors of industry, offering an excellent combination between thermal and mechanical properties. It is used in the automotive industry and electrical sectors. This product is available in colors on request.Information provided by Rhodia; Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.35 g/cc
0.0488 lb/in³
ISO 1183-A
Water Absorption 0.95 %
0.95 %
(Beginning Dry) 24 hours in water 23°C. ISO 62
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 110 MPa
16000 psi
ISO 527
Elongation at Break 4.5 %
4.5 %
ISO 527
Tensile Modulus 6.20 GPa
899 ksi
ISO 527
Flexural Yield Strength 170 MPa
24700 psi
ISO 178
Flexural Modulus 5.50 GPa
798 ksi
ISO 178
Izod Impact Resistance 2.40 J/cm²
11.4 ft-lb/in²
ISO 180
Charpy Impact Unnotched 10.8 J/cm²
51.4 ft-lb/in²
ISO 179/1EA-1993
Charpy Impact, Notched 3.15 J/cm²
15.0 ft-lb/in²
ISO 179/1EA-1993
Thermal Properties Metric English Comments
Melting Point 222 °C
432 °F
ISO 3146-C
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
IEC 93
Surface Resistance 1.00e+11 ohm
1.00e+11 ohm
IEC 93
Dielectric Constant 4.5

@Frequency 1e+6 Hz
4.5

@Frequency 1e+6 Hz
IEC 250
Dielectric Strength 22.0 kV/mm
559 kV/in
IEC 243-1
Dissipation Factor 0.090

@Frequency 1e+6 Hz
0.090

@Frequency 1e+6 Hz
IEC 250
Comparative Tracking Index 475 V
475 V
IEC 112
Processing Properties Metric English Comments
Rear Barrel Temperature 225 - 230 °C
437 - 446 °F
Middle Barrel Temperature 230 - 240 °C
446 - 464 °F
Front Barrel Temperature 240 - 250 °C
464 - 482 °F