Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Technyl Starâ„¢ S 60G1 V30 30% Glass Reinforced Nylon 6, Flame Retardant

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Glass Fiber Filled, Flame Retardant
Manufacturer Solvay
Trade Name Technyl Star™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Technyl Starâ„¢ S 60G1 V30 30% Glass Reinforced Nylon 6, Flame Retardant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This Halogen free flame retardant grade, based on high fluidity Technyl Star, combines excellent all-round mechanical properties with outstanding flame retardancy and electrical performance. This product is ideally suited for applications such as MCBs and contactors as well as being able to be used in many varied thin wall applications where its high flow polymer base enables it to achieve a UL94 V-0 rating down to a 0.4mm wall thickness. This product is available in a number of different colors including the standard Natural, light and dark Grey and Black. Specific colors and laser marking grades optimized for YAG and UV laser types are also available upon request.For all products containing Flame additives Rhodia recomends the use of high Chromium, low Carbon coating for the steels (example CR19% C1.9%). The use of this steel can help to prevent corrosion, extend the equipment lifetime and allow greater parameter flexibility.Information provided by Rhodia; Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.42 g/cc
0.0513 lb/in³
ISO 1183-A
Water Absorption 0.90 %

@Time 86400 sec
0.90 %

@Time 24.0 hour
ISO 62
Linear Mold Shrinkage, Flow 0.0040 cm/cm
0.0040 in/in
Rhodia EP test
Linear Mold Shrinkage, Transverse 0.0070 cm/cm
0.0070 in/in
Rhodia EP test
Mechanical Properties Metric English Comments
Tensile Strength at Break 97.0 MPa
14100 psi
Conditioned; ISO 527 Type 1 A
147 MPa
21300 psi
DAM; ISO 527 Type 1 A
Elongation at Break 2.28 %
2.28 %
DAM; ISO 527 Type 1 A
5.27 %
5.27 %
Conditioned; ISO 527 Type 1 A
Tensile Modulus 7.01 GPa
1020 ksi
Conditioned; ISO 527 Type 1 A
11.76 GPa
1706 ksi
DAM; ISO 527 Type 1 A
Flexural Strength 169 MPa
24500 psi
Conditioned; ISO 178
243 MPa
35200 psi
DAM; ISO 178
Flexural Modulus 6.90 GPa
1000 ksi
Conditioned; ISO 178
10.68 GPa
1549 ksi
DAM; ISO 178
Izod Impact, Notched (ISO) 9.00 kJ/m²
4.28 ft-lb/in²
DAM; ISO 180/A
12.0 kJ/m²
5.71 ft-lb/in²
Conditioned; ISO 180/A
Izod Impact, Unnotched (ISO) 54.0 kJ/m²
25.7 ft-lb/in²
DAM; ISO 180/1U
63.0 kJ/m²
30.0 ft-lb/in²
Conditioned; ISO 180/1U
Charpy Impact Unnotched 6.70 J/cm²
31.9 ft-lb/in²
DAM; ISO 179/1eU
6.90 J/cm²
32.8 ft-lb/in²
Conditioned; ISO 179/1eU
Charpy Impact, Notched 0.960 J/cm²
4.57 ft-lb/in²
DAM; ISO 179/1eA
1.30 J/cm²
6.19 ft-lb/in²
Conditioned; ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 222 °C
432 °F
ISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 205 °C
401 °F
ISO 75/Af
Flammability, UL94 V-0

@Thickness 0.381 mm
V-0

@Thickness 0.0150 in
DAM; ISO 1210/UL94
V-0

@Thickness 3.17 mm
V-0

@Thickness 0.125 in
DAM; ISO 1210/UL94
Oxygen Index 35 %
35 %
DAM; ISO 4589
Glow Wire Test 775 °C

@Thickness 20.3 mm
1430 °F

@Thickness 0.800 in
Glow Wire Ignition Temp; DAM; IEC 60695-2-13
800 °C

@Thickness 40.6 mm
1470 °F

@Thickness 1.60 in
Glow Wire Ignition Temp; DAM; IEC 60695-2-13
960 °C

@Thickness 20.3 mm
1760 °F

@Thickness 0.800 in
Glow Wire flammability Index; DAM; IEC 60695-2-12
960 °C

@Thickness 40.6 mm
1760 °F

@Thickness 1.60 in
Glow Wire flammability Index; DAM; IEC 60695-2-12
960 °C

@Thickness 81.3 mm
1760 °F

@Thickness 3.20 in
Glow Wire flammability Index; DAM; IEC 60695-2-12
Electrical Properties Metric English Comments
Surface Resistance 1.10e+14 ohm
1.10e+14 ohm
DAM; IEC 60093
Dielectric Constant 2.9
2.9
DAM; IEC 60250
4.35
4.35
Conditioned; IEC 60250
Dielectric Strength 28.5 kV/mm
724 kV/in
Conditioned; IEC 60243
39.8 kV/mm
1010 kV/in
DAM; IEC 60243
Dissipation Factor 0.080
0.080
Conditioned; IEC 60250
Comparative Tracking Index 600 V
600 V
DAM; IEC 60112
Processing Properties Metric English Comments
Rear Barrel Temperature 220 - 225 °C
428 - 437 °F
Middle Barrel Temperature 225 - 235 °C
437 - 455 °F
Front Barrel Temperature 235 - 245 °C
455 - 473 °F
Mold Temperature 80.0 °C
176 °F
Drying Temperature 80.0 °C
176 °F
Moisture Content <= 0.15 %
<= 0.15 %
Users viewing this material also viewed the following: