Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Spartech Formalloy HG High-Gloss TPO Alloy Specialty Sheet

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Olefinic Elastomer (TPO) , TPO
Manufacturer Spartech
Trade Name Formalloy
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Spartech Formalloy HG High-Gloss TPO Alloy Specialty Sheet.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Specialty SheetInformation provided by Spartech.
Physical Properties Metric English Comments
Specific Gravity 1.07 g/cc
1.07 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 30.3 MPa
4400 psi
ASTM D638
Tensile Strength, Yield 23.4 MPa
3400 psi
ASTM D638
Elongation at Break 400 %
400 %
ASTM D638
Flexural Modulus 1.10 GPa
160 ksi
ASTM D790
Thermal Properties Metric English Comments
CTE, linear 108 µm/m-°C

@Temperature 20.0 °C
60.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 82.2 °C
180 °F
ASTM D648
Optical Properties Metric English Comments
Gloss 80 - 85 %
80 - 85 %
Gardner; ASTM D2523
Users viewing this material also viewed the following: