Material Notes:
Description: Weatherable SheetGeloy is a registered trademark of General Electric Company.Information provided by Spartech.
Physical Properties Metric English Comments
Specific Gravity 1.05 g/cc
1.05 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 88
88
ASTM D785
Tensile Strength, Yield 32.4 MPa
4700 psi
ASTM D638
Tensile Modulus 1.93 GPa
280 ksi
ASTM D638
Flexural Yield Strength 51.7 MPa
7500 psi
ASTM D790
Flexural Modulus 1.93 GPa
280 ksi
ASTM D790
Izod Impact, Unnotched 3.74 J/cm
7.00 ft-lb/in
ASTM D256
0.854 J/cm

@Temperature -40.0 °C
1.60 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Falling Dart Impact 29.8 J
22.0 ft-lb
73°F; ASTM D3029
19.0 J

@Temperature -40.0 °C
14.0 ft-lb

@Temperature -40.0 °F
ASTM D3029
Thermal Properties Metric English Comments
CTE, linear 90.0 µm/m-°C

@Temperature 20.0 °C
50.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 79.4 °C
175 °F
ASTM D648
Flammability, UL94 HB
HB
Optical Properties Metric English Comments
Gloss 90 %
90 %
Gardner; ASTM D2523