Spartech PP5930 Glass/Mica Reinforced Homopolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 30% Mica Filler
Manufacturer Spartech
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Spartech PP5930 Glass/Mica Reinforced Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Spartech
Physical Properties Metric English Comments
Specific Gravity 1.14 g/cc

@Temperature 22.8 °C
1.14 g/cc

@Temperature 73.0 °F
ASTM D792
Filler Content 30 %
30 %
Glass/Mica
Linear Mold Shrinkage 0.0040 cm/cm
0.0040 in/in
0.125inch wall
Mechanical Properties Metric English Comments
Tensile Strength, Yield 41.4 MPa
6000 psi
ASTM D638
Elongation at Break 2.5 %
2.5 %
ASTM D638
Elongation at Yield 2.0 %
2.0 %
ASTM D638
Flexural Modulus 3.79 GPa
550 ksi
secant; ASTM D790
5.52 GPa
800 ksi
tangent; ASTM D790
Izod Impact, Notched 0.534 J/cm

@Temperature 22.8 °C
1.00 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 149 °C
300 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 127 °C
260 °F
ASTM D648