Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Spartech Polycast SP 1.25 Cell Cast Acrylic

Category Polymer , Thermoplastic , Acrylic (PMMA)
Manufacturer Spartech
Trade Name Polycast
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Spartech Polycast SP 1.25 Cell Cast Acrylic.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Cell Cast AcrylicInformation provided by Spartech.
Physical Properties Metric English Comments
Water Absorption 0.20 %
0.20 %
24 hr immersion
Mechanical Properties Metric English Comments
Tensile Strength, Yield 64.8 MPa
9400 psi
ASTM D638
Tensile Modulus 2.76 GPa
400 ksi
ASTM D638
Compressive Modulus 2.76 GPa
400 ksi
ASTM D695
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 76.7 °C
170 °F
Minimum Service Temperature, Air -32.2 °C
-26.0 °F
Lowest Temp Tested for Bullet Resistance
Flame Spread 5.8 mm/min
0.23 in/min
Burning Rate UL 94 HB; ASTM D635
Optical Properties Metric English Comments
Haze <= 1.5 %
<= 1.5 %
As Cast; ASTM D1003
Yellow Index <= 1.0 %
<= 1.0 %
As Cast; ASTM D1925
Transmission, Visible >= 85 %
>= 85 %
As Cast; ASTM D1003
UV Transmittance 0.00 %

@Wavelength 320 nm
0.00 %

@Wavelength 320 nm
Descriptive Properties Value Comments
Ballistic Protection .44 Magnum
Smoke Density Max 65%; Rating 49%
ASTM D2843
Users viewing this material also viewed the following: