Spartech SP-1010 Polyolefin Sheet

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , Polyolefin
Manufacturer Spartech
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Spartech SP-1010 Polyolefin Sheet.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Polyolefin SheetInformation provided by Spartech.
Physical Properties Metric English Comments
Specific Gravity 0.960 g/cc
0.960 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 66
66
ASTM D2240
Tensile Strength, Yield 31.0 MPa
4500 psi
ASTM D638
Elongation at Break 800 %
800 %
ASTM D638
Tensile Modulus 0.655 GPa
95.0 ksi
ASTM D638
Flexural Modulus 1.55 GPa
225 ksi
ASTM D790
Izod Impact, Unnotched 2.14 J/cm
4.00 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 108 µm/m-°C

@Temperature 20.0 °C
60.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 80.0 °C
176 °F
ASTM D648
Flammability, UL94 HB
HB