Spartech Spectar® Copolyester Sheet

Category Polymer , Thermoplastic , Polyester, TP
Manufacturer Spartech
Trade Name Spectar®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Spartech Spectar® Copolyester Sheet.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Copolyester SheetSpectar is a registered trademark of Eastman Chemical Company.Information provided by Spartech.
Physical Properties Metric English Comments
Specific Gravity 1.27 g/cc
1.27 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 115
115
ASTM D785
Tensile Strength, Yield 53.1 MPa
7700 psi
ASTM D638
Tensile Modulus 2.21 GPa
320 ksi
ASTM D638
Flexural Yield Strength 77.2 MPa
11200 psi
ASTM D790
Flexural Modulus 2.14 GPa
310 ksi
ASTM D790
Izod Impact, Unnotched 0.908 J/cm
1.70 ft-lb/in
ASTM D256
0.374 J/cm

@Temperature -40.0 °C
0.700 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 72.0 µm/m-°C

@Temperature 20.0 °C
40.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 73.9 °C
165 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C
158 °F
ASTM D648
Flammability, UL94 HB
HB