Spartech Spectrum® S370 TPO Polyolefin Sheet  (discontinued **)

Category Polymer , Thermoplastic , Polyolefin
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Spartech Spectrum® S370 TPO Polyolefin Sheet  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer.
Physical Properties Metric English Comments
Density 0.920 g/cc
0.0332 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell R 58
58
Tensile Strength, Ultimate 16.5 MPa
2390 psi
Machine direction
Flexural Yield Strength 18.6 MPa
2700 psi
Flexural Modulus 0.700 GPa
102 ksi
Izod Impact, Notched 5.30 J/cm
9.93 ft-lb/in
1.30 J/cm

@Temperature -29.0 °C
2.44 ft-lb/in

@Temperature -20.2 °F
Gardner Impact >= 36.0 J
>= 26.6 ft-lb
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 66.0 °C
151 °F