Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Special Metals Electroformed Nickel, 6 Micron (0.24 mil) Foil, As-Electroformed

Category Metal , Nonferrous Metal , Nickel Alloy , Pure Element
Manufacturer Special Metals (includes the former Inco Alloys International Inc.)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Special Metals Electroformed Nickel, 6 Micron (0.24 mil) Foil, As-Electroformed.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer, Special Metals.
Physical Properties Metric English Comments
Density 8.91 g/cc
0.322 lb/in³
Thickness 6.10 microns
0.240 mil
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 827 MPa
120000 psi
Elongation at Break <= 0.50 %
<= 0.50 %
Component Elements Properties Metric English Comments
Carbon, C <= 0.010 %
<= 0.010 %
Chromium, Cr <= 0.010 %
<= 0.010 %
Cobalt, Co <= 0.010 %
<= 0.010 %
Copper, Cu <= 0.010 %
<= 0.010 %
Iron, Fe <= 0.010 %
<= 0.010 %
Nickel, Ni >= 99.95 %
>= 99.95 %
Sulfur, S <= 0.0020 %
<= 0.0020 %
Zinc, Zn <= 0.0010 %
<= 0.0010 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000800 ohm-cm
0.00000800 ohm-cm
Users viewing this material also viewed the following: