Material Notes:
A mechanically alloyed nickel-chromium alloy with oxide dispersion strengthening. Mechanical alloying, which involves high-energy milling of metal powders, is used to create a uniformly distributed, fine dispersoid of yttrium oxide in the alloy. The dispersoid, which is stable to the alloy's melting point, imparts exceptional high-temperature strength and creep resistance. The alloy's strength, corrosion resistance, and microstructural stability make it useful for gas-turbine vanes and other extreme-service applications. Standard product forms are round, flats, extruded section, plate, and wire.Data provided by the manufacturer, Special Metals.
Physical Properties Metric English Comments
Density 8.30 g/cc
0.300 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 950 MPa
138000 psi
Annealed
730 MPa

@Temperature 550 °C
106000 psi

@Temperature 1020 °F
Annealed prior to test
Tensile Strength, Yield 570 MPa
82700 psi
Annealed
500 MPa

@Temperature 550 °C
72500 psi

@Temperature 1020 °F
Annealed prior to test
Elongation at Break 20 %
20 %
Annealed prior to test.
18 %

@Temperature 550 °C
18 %

@Temperature 1020 °F
Annealed prior to test.
Thermal Properties Metric English Comments
CTE, linear 12.2 µm/m-°C

@Temperature 20.0 - 100 °C
6.78 µin/in-°F

@Temperature 68.0 - 212 °F
Thermal Conductivity 14.26 W/m-K
98.96 BTU-in/hr-ft²-°F
Melting Point 1400 °C
2550 °F
Component Elements Properties Metric English Comments
Aluminum, Al 0.30 %
0.30 %
Carbon, C 0.050 %
0.050 %
Chromium, Cr 20 %
20 %
Iron, Fe 1.0 %
1.0 %
Nickel, Ni 78 %
78 %
Titanium, Ti 0.50 %
0.50 %
Y2O3 0.60 %
0.60 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0001075 ohm-cm
0.0001075 ohm-cm
Magnetic Permeability 1.001
1.001
at 200 oersted (15.9 kA/m)