Material Notes:
A nickel-chromium alloy with good mechanical properties and oxidation resistance at high temperatures. Used for sheet-metal fabrications in gas-turbine engines, for components of industrial furnaces, for heat-treating equipment and fixtures, and in nuclear engineering. Standard product forms are round, hexagon, flats, extruded section, tube, pipe, plate, sheet, strip, and wire.Data provided by the manufacturer, Special Metals.
Physical Properties Metric English Comments
Density 8.37 g/cc
0.302 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 750 MPa
109000 psi
Annealed
660 MPa

@Temperature 550 °C
95700 psi

@Temperature 1020 °F
Annealed prior to test
Tensile Strength, Yield 275 MPa
39900 psi
Annealed
210 MPa

@Temperature 550 °C
30500 psi

@Temperature 1020 °F
Annealed prior to test
Elongation at Break 42 %
42 %
Annealed prior to test.
40 %

@Temperature 550 °C
40 %

@Temperature 1020 °F
Annealed prior to test.
Thermal Properties Metric English Comments
CTE, linear 11.0 µm/m-°C

@Temperature 20.0 - 100 °C
6.11 µin/in-°F

@Temperature 68.0 - 212 °F
Specific Heat Capacity 0.461 J/g-°C
0.110 BTU/lb-°F
Thermal Conductivity 11.7 W/m-K
81.2 BTU-in/hr-ft²-°F
Melting Point 1340 - 1380 °C
2440 - 2520 °F
Solidus 1340 °C
2440 °F
Liquidus 1380 °C
2520 °F
Component Elements Properties Metric English Comments
Carbon, C 0.080 - 0.15 %
0.080 - 0.15 %
Chromium, Cr 18 - 21 %
18 - 21 %
Copper, Cu <= 0.50 %
<= 0.50 %
Iron, Fe <= 5.0 %
<= 5.0 %
Manganese, Mn <= 1.0 %
<= 1.0 %
Nickel, Ni 72 %
72 %
As remainder
Silicon, Si <= 1.0 %
<= 1.0 %
Titanium, Ti 0.20 - 0.60 %
0.20 - 0.60 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.000109 ohm-cm
0.000109 ohm-cm