Material Notes:
Wrought nickel similar to Nickel 200 but with compositional adjustments to enhance performance in electrical and electronic applications. Ferromagnetic. Used for the anodes and grids of electronic valves, magnetostrictive transducers, lead wires, transistor housings, and battery cases. Standard product forms are sheet, strip and wire.Data provided by the manufacturer, Special Metals.
Physical Properties Metric English Comments
Density 8.89 g/cc
0.321 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 345 MPa
50000 psi
Annealed
Tensile Strength, Yield 90.0 MPa

@Strain 0.200 %
13100 psi

@Strain 0.200 %
Annealed
Elongation at Break 45 %
45 %
Annealed
Thermal Properties Metric English Comments
CTE, linear 13.3 µm/m-°C

@Temperature 20.0 - 100 °C
7.39 µin/in-°F

@Temperature 68.0 - 212 °F
Specific Heat Capacity 0.456 J/g-°C
0.109 BTU/lb-°F
Thermal Conductivity 75.0 W/m-K
521 BTU-in/hr-ft²-°F
Melting Point 1435 - 1446 °C
2615 - 2635 °F
Solidus 1435 °C
2615 °F
Liquidus 1446 °C
2635 °F
Component Elements Properties Metric English Comments
Carbon, C <= 0.15 %
<= 0.15 %
Copper, Cu <= 0.15 %
<= 0.15 %
Iron, Fe <= 0.20 %
<= 0.20 %
Magnesium, Mg 0.010 - 0.080 %
0.010 - 0.080 %
Manganese, Mn <= 0.35 %
<= 0.35 %
Nickel, Ni >= 99 %
>= 99 %
Including Cobalt
Silicon, Si <= 0.15 %
<= 0.15 %
Sulfur, S <= 0.0080 %
<= 0.0080 %
Titanium, Ti 0.010 - 0.050 %
0.010 - 0.050 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000950 ohm-cm
0.00000950 ohm-cm
Curie Temperature 360 °C
680 °F