Material Notes:
A high-purity grade of nickel made by powder metallurgy. It has a low base hardness and high ductility. Its extreme purity is useful for components of hydrogen thyratrons. It is also used for electrical resistance thermometers. Ferromagnetic. Standard product forms are round, plate, sheet, strip, tube, and wire.Data provided by the manufacturer, Special Metals.
Physical Properties Metric English Comments
Density 8.89 g/cc
0.321 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 345 MPa
50000 psi
Annealed
Tensile Strength, Yield 110 MPa

@Strain 0.200 %
16000 psi

@Strain 0.200 %
Annealed
Elongation at Break 50 %
50 %
Annealed
Thermal Properties Metric English Comments
CTE, linear 13.3 µm/m-°C

@Temperature 20.0 - 100 °C
7.39 µin/in-°F

@Temperature 68.0 - 212 °F
Specific Heat Capacity 0.460 J/g-°C
0.110 BTU/lb-°F
Thermal Conductivity 86.0 W/m-K
597 BTU-in/hr-ft²-°F
Melting Point 1454 °C
2649 °F
Component Elements Properties Metric English Comments
Carbon, C <= 0.020 %
<= 0.020 %
Copper, Cu <= 0.010 %
<= 0.010 %
Iron, Fe <= 0.050 %
<= 0.050 %
Magnesium, Mg <= 0.0050 %
<= 0.0050 %
Manganese, Mn <= 0.0030 %
<= 0.0030 %
Nickel, Ni >= 99.9 %
>= 99.9 %
Including Cobalt
Silicon, Si <= 0.0050 %
<= 0.0050 %
Sulfur, S <= 0.0030 %
<= 0.0030 %
Titanium, Ti <= 0.0050 %
<= 0.0050 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000750 ohm-cm
0.00000750 ohm-cm