Specialty Materials Boron Monofilament

Category Metal , Other Engineering Material , Composite Fibers , Pure Element
Manufacturer Specialty Materials, Inc.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Specialty Materials Boron Monofilament.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Exceptional compression strength. Specialty Materials' Chemical Vapor Deposition process uses fine tungsten wire for the substrate and boron trichloride gas as the boron source.Information provided by Specialty Materials, Inc.
Physical Properties Metric English Comments
Density 2.57 g/cc
0.0928 lb/in³
Mechanical Properties Metric English Comments
Hardness, Knoop 3200
3200
Tensile Strength, Ultimate 3600 MPa
522000 psi
Elongation at Yield 0.90 %
0.90 %
Modulus of Elasticity 400 GPa
58000 ksi
Thermal Properties Metric English Comments
CTE, linear 4.50 µm/m-°C

@Temperature 20.0 °C
2.50 µin/in-°F

@Temperature 68.0 °F
Specific Heat Capacity 1.00 J/g-°C
0.239 BTU/lb-°F
Thermal Conductivity 25.0 W/m-K
174 BTU-in/hr-ft²-°F
Melting Point 2300 °C
4170 °F
Maximum Service Temperature, Air 500 °C
932 °F
Component Elements Properties Metric English Comments
Boron, B 100 %
100 %
Electrical Properties Metric English Comments
Electrical Resistivity 250 ohm-cm
250 ohm-cm
Processing Properties Metric English Comments
Processing Temperature 1350 °C
2460 °F