Stratasys® ABSplus

Category Polymer , Rapid Prototyping Polymer , Thermoplastic , ABS Polymer
Manufacturer Stratasys
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Stratasys® ABSplus.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ABSplus is up to 40 percent stronger than standard ABS material and is an ideal material for conceptual prototyping through design verification through direct digital manufacturing. The marriage of ABSplus with FDM technology gives you the ability to create Real Parts™ direct from digital files that are stronger, smoother, and with more feature detail.Information provided by Stratasys®
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 36.0 MPa
5220 psi
Type 1, 2"/min; ASTM D638
Elongation at Break 4.0 %
4.0 %
ASTM D638
Tensile Modulus 2.265 GPa
328.5 ksi
Type 1, 2"/min; ASTM D638
Flexural Strength 52.0 MPa
7540 psi
ASTM D790
Flexural Modulus 2.198 GPa
318.8 ksi
ASTM D790
Izod Impact, Notched 0.960 J/cm
1.80 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 88.2 µm/m-°C

@Temperature 20.0 °C
49.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 96.0 °C
205 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 82.0 °C
180 °F
ASTM D648