Struktol TPW 609 Processing Additive

Category Other Engineering Material , Additive/Filler for Polymer , Polymer
Manufacturer Struktol
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Struktol TPW 609 Processing Additive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Blend of complex, modified fatty acid ester.Applications: STRUKTOL® TPW 609 has shown excellent results in producing extruded polymer / wood composites with or without coupling agents at a lower dosage than other lubricants on the market. STRUKTOL® TPW 609 offers very good mixing, improved filler dispersion and improved extrusion rates.Information provided by Struktol
Physical Properties Metric English Comments
Specific Gravity 1.00 g/cc
1.00 g/cc
Additive Loading 1.0 - 2.0 %
1.0 - 2.0 %
in PP/wood formulas
3.0 - 4.0 %
3.0 - 4.0 %
In HDPE/wood applications
Thermal Properties Metric English Comments
Dropping Point 114 - 154 °C
237 - 309 °F
Processing Properties Metric English Comments
Shelf Life >= 24.0 Month
>= 24.0 Month
Descriptive Properties Value Comments
Appearance Beige pastille and powder