Styrolution Luran® VLN SAN

Category Polymer , Thermoplastic , SAN Polymer , Styrene Acrylonitrile (SAN), Transparent
Manufacturer Styrolution
Trade Name Luran®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Styrolution Luran® VLN SAN.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Luran® VLN is a styrene/acrylonitrile copolymer without any lubricants particularly suitable for ABS compounds. Luran® VLN is an easy flowing SAN grade especially suited for injection molding ABS compounds. Due to its low acrylonitrile content, ABS compounds with good compatibility to polycarbonate are accessible.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS
Thermal Properties Metric English Comments
Vicat Softening Point 100 °C
212 °F
VST B50; ISO 306
Descriptive Properties Value Comments
Color Natural