Styrolution PS 5410 HIPS

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Impact Modified
Manufacturer Styrolution
Trade Name PS
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Styrolution PS 5410 HIPS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Good printabilityGood environmental stress crack resistanceLow GelsTrims CleanlyLow Gloss (matte finish)Information provided by Styrolution
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ASTM D 792
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
0.0040 - 0.0070 in/in
ASTM D 955
Melt Flow 3.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
3.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D 1238
Mechanical Properties Metric English Comments
Hardness, Rockwell L 50
50
ASTM D 785
Tensile Strength, Yield 17.2 MPa
2500 psi
ASTM D 638
Elongation at Break 50 %
50 %
ASTM D 638
Tensile Modulus 1.69 GPa
245 ksi
ASTM D 638
Flexural Strength 37.9 MPa
5500 psi
ASTM D 790
Flexural Modulus 1.69 GPa
245 ksi
ASTM D 790
Izod Impact, Notched 1.49 J/cm
2.80 ft-lb/in
ASTM D 638
Thermal Properties Metric English Comments
CTE, linear 90.0 µm/m-°C
50.0 µin/in-°F
ASTM D 696
Vicat Softening Point 98.9 °C

@Load 1.02 kg
210 °F

@Load 2.25 lb
120°C/h; ASTM D 1525
Optical Properties Metric English Comments
Gloss 15 %
15 %
Specular Gloss, 60°; ASTM D 523
Electrical Properties Metric English Comments
Dielectric Constant 2.5

@Thickness 1.00 mm,
Frequency 1.00e+6 Hz
2.5

@Thickness 0.0394 in,
Frequency 1.00e+6 Hz
ASTM D 150
Dielectric Strength 15.7 kV/mm
400 kV/in
ASTM D 696