Material Notes:
Description: Polystyrol 165 H is a high molecular weight, good flowing grade, often blended with high impact extrusion grades.Applications: In blends with high impact Polystyrene or Styrolux; thermoformed articles for high impact resistant packagings of dairy products, breakers for cold beverages. As material for physically or chemically foamed sheet, eg. for meat trays or labels.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS
Physical Properties Metric English Comments
Density 1.045 g/cc
0.03775 lb/in³
ISO 1183
Water Absorption <= 0.10 %
<= 0.10 %
ISO 62
Moisture Absorption at Equilibrium <= 0.10 %
<= 0.10 %
23°C/50% RH; ISO 62
Melt Flow 3.553 g/10 min

@Load 5.00 kg,
Temperature 200 °C
3.553 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ISO 1133
Mechanical Properties Metric English Comments
Ball Indentation Hardness 150 MPa

@Load 36.5 kg,
Time 30.0 sec
21800 psi

@Load 80.5 lb,
Time 0.00833 hour
ISO 2039-1
Tensile Strength at Break 52.0 MPa
7540 psi
ISO 527-1/-2
Elongation at Break 2.0 %
2.0 %
ISO 527-1/-2
Tensile Modulus 3.30 GPa
479 ksi
ISO 527-1/-2
Flexural Strength 86.0 MPa
12500 psi
ISO 178
Shear Modulus 1.40 GPa
203 ksi
ISO 6721-2
Charpy Impact Unnotched <= 2.50 J/cm²
<= 11.9 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 0.300 J/cm²
1.43 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 84.0 °C
183 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 76.0 °C
169 °F
ISO 75-1/-2
Vicat Softening Point 89.0 °C
192 °F
VST/B/50; ISO 306
97.0 °C
207 °F
VST/A/120; ISO 306
Flammability, UL94 HB

@Diameter 1.60 mm
HB

@Diameter 0.0630 in
IEC 60695-11-10
HB

@Diameter 3.18 mm
HB

@Diameter 0.125 in
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+16 ohm-cm
>= 1.00e+16 ohm-cm
IEC 60093
Surface Resistance >= 1.00e+14 ohm
>= 1.00e+14 ohm
IEC 60093
Dielectric Constant 2.5

@Frequency 1.00e+6 Hz
2.5

@Frequency 1.00e+6 Hz
IEC 60250
2.5

@Frequency 100 Hz
2.5

@Frequency 100 Hz
IEC 60250
Dielectric Strength 135 kV/mm
3430 kV/in
K20/P50; IEC 60243-1
Processing Properties Metric English Comments
Melt Temperature 200 - 240 °C
392 - 464 °F
Flat film
180 - 280 °C
356 - 536 °F
Injection Molding
Mold Temperature 10.0 - 60.0 °C
50.0 - 140 °F
Injection Molding
Descriptive Properties Value Comments
Color Crystal Clear 00013
Commercial Status Europe
Primary Processing Technique Injection Molding and Extrusion