Material Notes:
Description: Styrolux® 693 D is a clear styrene-butadiene copolymer (SBC) with a well balanced combination of toughness and clarity. Styrolux® 693 D is mainly used for thermoformed articles, especially in blends with general-purpose polystyrene. Styrolux® 693 D contains a microcrystalline wax which acts as an antiblock providing processing benefits but decreases the printability.Major applications include: food and non-food packagings, thermoformed transparent containers and cups for cold beverages, thermoformed lids, toys and boxes.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS
Physical Properties Metric English Comments
Density 1.01 g/cc
0.0365 lb/in³
ISO 1183
Water Absorption <= 0.070 %
<= 0.070 %
ISO 62
Moisture Absorption at Equilibrium <= 0.070 %
<= 0.070 %
23°C/50% RH; ISO 62
Melt Flow 12.63 g/10 min
12.63 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 64
64
ISO 868
Tensile Strength, Yield 22.0 MPa
3190 psi
ISO 527-1/-2
Elongation at Break 260 %
260 %
Nominal; ISO 527-1/-2
Elongation at Yield 2.2 %
2.2 %
ISO 527-1/-2
Tensile Modulus 1.30 GPa
189 ksi
ISO 527-1/-2
Flexural Strength 32.0 MPa
4640 psi
ISO 178
Flexural Modulus 1.40 GPa
203 ksi
ASTM D790
Izod Impact, Notched 0.350 J/cm
0.656 ft-lb/in
ASTM D256
Izod Impact, Notched (ISO) 2.80 kJ/m²

@Temperature -30.0 °C
1.33 ft-lb/in²

@Temperature -22.0 °F
ISO 180/A
3.50 kJ/m²

@Temperature 23.0 °C
1.67 ft-lb/in²

@Temperature 73.4 °F
ISO 180/A
Charpy Impact Unnotched <= NB
<= NB
ISO 179/1eU
Charpy Impact, Notched 0.500 J/cm²
2.38 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 72.0 °C
162 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 59.0 °C
138 °F
ISO 75-1/-2
Vicat Softening Point 48.0 °C
118 °F
VST/B/50; ISO 306
76.0 °C
169 °F
VST/A/50; ISO 306
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
IEC 60695-11-10
HB

@Thickness 3.18 mm
HB

@Thickness 0.125 in
IEC 60695-11-10
Optical Properties Metric English Comments
Haze 2.0 %
2.0 %
DIN 5036-3
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+13 ohm-cm
>= 1.00e+13 ohm-cm
IEC 60093
Surface Resistance 1.00e+15 ohm
1.00e+15 ohm
IEC 60093
Dielectric Constant 2.5

@Frequency 1.00e+6 Hz
2.5

@Frequency 1.00e+6 Hz
IEC 60250
2.5

@Frequency 100 Hz
2.5

@Frequency 100 Hz
IEC 60250
Dielectric Strength 88.0 kV/mm
2240 kV/in
K20/P50; IEC 60243-1
Processing Properties Metric English Comments
Melt Temperature 190 - 230 °C
374 - 446 °F
Flat film extrusion
180 - 250 °C
356 - 482 °F
Injection molding
Mold Temperature 20.0 - 40.0 °C
68.0 - 104 °F
Injection Molding
Descriptive Properties Value Comments
Color Crystal Clear
Commercial Status Europe
Primary Processing Technique Injection Molding, Extrusion, and Blow Molding
Transparency 0.89
d=2mm, DIN 5036-3
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved