Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Styrolution Terblend® N NM-21 EF Gray 38058 ABS+PA (Conditioned)

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend , Nylon
Manufacturer Styrolution
Trade Name Terblend®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Styrolution Terblend® N NM-21 EF Gray 38058 ABS+PA (Conditioned).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Terblend® N NM-21 EF is an UV stabilized ABS/PA blend combining very high impact strength, even at low temperatures. The enhanced flowability enables excellent processability and surface appearance.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS
Physical Properties Metric English Comments
Density 1.07 g/cc
0.0387 lb/in³
ISO 1183
Moisture Absorption at Equilibrium 1.3 %
1.3 %
23°C/50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0070 cm/cm
0.0070 in/in
ISO 2577
Melt Flow 64.2 g/10 min

@Load 10.0 kg,
Temperature 240 °C
64.2 g/10 min

@Load 22.0 lb,
Temperature 464 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Rockwell R 103
103
ISO 2039-2
Tensile Strength, Yield 36.0 MPa
5220 psi
ISO 527-1/-2
Elongation at Break 50 %
50 %
Nominal; ISO 527-1/-2
Elongation at Yield 5.0 %
5.0 %
ISO 527-1/-2
Tensile Modulus 1.40 GPa
203 ksi
ISO 527-1/-2
Izod Impact, Notched (ISO) 9.00 kJ/m²

@Temperature -30.0 °C
4.28 ft-lb/in²

@Temperature -22.0 °F
ISO 180/A
80.0 kJ/m²

@Temperature 23.0 °C
38.1 ft-lb/in²

@Temperature 73.4 °F
ISO 180/A
Charpy Impact Unnotched NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
ISO 179/1eU
NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 1.00 J/cm²

@Temperature -30.0 °C
4.76 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
8.50 J/cm²

@Temperature 23.0 °C
40.4 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Vicat Softening Point 110 °C
230 °F
VST/B/50; ISO 306
200 °C
392 °F
VST/A/50; ISO 306
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
IEC 60093
Dielectric Constant 3.8

@Frequency 1.00e+6 Hz
3.8

@Frequency 1.00e+6 Hz
IEC 60250
Dissipation Factor 0.090

@Frequency 1.00e+6 Hz
0.090

@Frequency 1.00e+6 Hz
IEC 60250
Processing Properties Metric English Comments
Melt Temperature 240 - 270 °C
464 - 518 °F
Injection Molding
Mold Temperature 40.0 - 80.0 °C
104 - 176 °F
Injection Molding
Descriptive Properties Value Comments
Color Gray 38058
Commercial Status Europe
Primary Processing Technique Injection Molding and Extrusion