Styrolution Terlux® 2812 HD MABS

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded
Manufacturer Styrolution
Trade Name Terlux®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Styrolution Terlux® 2812 HD MABS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Terlux 2812 HD is a suitable grade for the food packaging and health care and diagnostic markets.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
ISO 1183
Moisture Absorption at Equilibrium 0.35 %
0.35 %
50% RH; ISO 62
0.70 %
0.70 %
Saturation; ISO 62
Linear Mold Shrinkage, Flow 0.0055 cm/cm
0.0055 in/in
ISO 294-4
Melt Flow 8.64 g/10 min

@Load 10.0 kg,
Temperature 220 °C
8.64 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ISO 1133
Mechanical Properties Metric English Comments
Ball Indentation Hardness 75.0 MPa

@Load 36.5 kg,
Time 30.0 sec
10900 psi

@Load 80.5 lb,
Time 0.00833 hour
ISO 2039-1
Tensile Strength, Yield 42.0 MPa
6090 psi
ISO 527-1/-2
Elongation at Break 20 %
20 %
Nominal; ISO 527
Elongation at Yield 4.0 %
4.0 %
ISO 52
Tensile Modulus 1.90 GPa
276 ksi
ISO 527
Charpy Impact Unnotched 8.00 J/cm²

@Temperature -30.0 °C
38.1 ft-lb/in²

@Temperature -22.0 °F
ISO 179
12.0 J/cm²

@Temperature 23.0 °C
57.1 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Charpy Impact, Notched 0.200 J/cm²

@Temperature -30.0 °C
0.952 ft-lb/in²

@Temperature -22.0 °F
ISO 179
0.500 J/cm²

@Temperature 23.0 °C
2.38 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 95.0 µm/m-°C
52.8 µin/in-°F
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C
194 °F
ISO 75
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+13 ohm-cm
>= 1.00e+13 ohm-cm
IEC 60093
Surface Resistance 1.00e+15 ohm
1.00e+15 ohm
IEC 60093
Dielectric Constant 2.8

@Frequency 1.00e+6 Hz
2.8

@Frequency 1.00e+6 Hz
IEC 60250
3.0

@Frequency 100 Hz
3.0

@Frequency 100 Hz
IEC 60250
Dielectric Strength 37.0 kV/mm
940 kV/in
K20/P50; IEC 60243-1
Dissipation Factor 0.013

@Frequency 1.00e+6 Hz
0.013

@Frequency 1.00e+6 Hz
IEC 60250
0.016

@Frequency 100 Hz
0.016

@Frequency 100 Hz
IEC 60250
Descriptive Properties Value Comments
Commercial Status North America