Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Styron CALIBREâ„¢ 303-6 Polycarbonate Resin

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer Styron
Trade Name CALIBRE™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Styron CALIBREâ„¢ 303-6 Polycarbonate Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Overview: CALIBREâ„¢ 300-6 polycarbonate resins offer exceptional impact resistance, heat distortion resistance and optical clarity as well as high melt strength for blow molding and sheet applications. The CALIBREâ„¢ 300-6 series products are available in 4 additive packages: CALIBREâ„¢ 300: No mold release or UV Stabilizer. CALIBREâ„¢ 301: Mold release. CALIBREâ„¢ 302: UV stabilizer. CALIBREâ„¢ 303: Mold release and UV stabilizer.Applications:Automotive interiorsAutomotive exteriorsSheet applicationsElectrical lighting/switchesSmall & large appliancesBeverage containers/servicewarePower equipmentGovt. and Industry Standards:CSAUnderwriters Laboratory (UL) Information provided by Styron
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ISO 1183/A
Water Absorption 0.32 %

@Temperature 23.0 °C
0.32 %

@Temperature 73.4 °F
Equilibrium, 50% RH; ISO 62
0.15 %

@Temperature 23.0 °C,
Time 86400 sec
0.15 %

@Temperature 73.4 °F,
Time 24.0 hour
ISO 62
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
ISO 294-4
Melt Flow 6.0 g/10 min

@Load 1.20 kg,
Temperature 300 °C
6.0 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Rockwell M 73
73
ASTM D785
Hardness, Rockwell R 118
118
ASTM D785
Tensile Strength at Break 72.0 MPa
10400 psi
ISO 527-2/50
Tensile Strength, Yield 60.0 MPa
8700 psi
ISO 527-2/50
Elongation at Break 150 %
150 %
ISO 527-2/50
Elongation at Yield 6.0 %
6.0 %
ISO 527-2/50
Tensile Modulus 2.30 GPa
334 ksi
ISO 527-2/50
Flexural Strength 97.0 MPa
14100 psi
2.0 mm/min; ISO 178
Flexural Modulus 2.40 GPa
348 ksi
2.0 mm/min; ISO 178
Izod Impact, Unnotched (ISO) 93.0 kJ/m²

@Temperature 23.0 °C
44.3 ft-lb/in²

@Temperature 73.4 °F
ISO 180/A
Charpy Impact, Notched 1.40 J/cm²

@Temperature -30.0 °C
6.66 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
5.50 J/cm²

@Temperature 12.0 °C
26.2 ft-lb/in²

@Temperature 53.6 °F
ISO 179/1eA
Abrasion 45
45
[%] Taber; ISO 9352
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 70.0 µm/m-°C
38.9 µin/in-°F
ISO 11359-2
Hot Ball Pressure Test >= 125 °C
>= 257 °F
IEC 60335-1
Deflection Temperature at 0.46 MPa (66 psi) 146 °C
295 °F
Annealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 126 °C
259 °F
Unannealed; ISO 75-2/A
143 °C
289 °F
Annealed; ISO 75-2/A
Vicat Softening Point 151 °C
304 °F
ISO 306/B50
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in
Oxygen Index 26 %
26 %
ISO 4289-2
Glow Wire Test 875 °C

@Thickness 2.00 mm
1610 °F

@Thickness 0.0787 in
IEC 60695-2-12
875 °C

@Thickness 3.00 mm
1610 °F

@Thickness 0.118 in
IEC 60695-2-12
900 °C

@Thickness 1.00 mm
1650 °F

@Thickness 0.0394 in
IEC 60695-2-12
Optical Properties Metric English Comments
Refractive Index 1.586
1.586
ASTM D542; ISO 489
Haze 1.0 %
1.0 %
ASTM D1003
Transmission, Visible 89 %
89 %
ASTM D1003
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
IEC 60093
Dielectric Constant 3.0

@Frequency 60.0 Hz
3.0

@Frequency 60.0 Hz
IEC 60250
3.0

@Frequency 1.00e+6 Hz
3.0

@Frequency 1.00e+6 Hz
IEC 60250
3.0

@Frequency 100 Hz
3.0

@Frequency 100 Hz
IEC 60250
Dielectric Strength 17.0 kV/mm
432 kV/in
IEC 60243-1
Dissipation Factor 0.0010

@Frequency 50.0 Hz
0.0010

@Frequency 50.0 Hz
ASTM D150
0.0020

@Frequency 1.00e+6 Hz
0.0020

@Frequency 1.00e+6 Hz
ASTM D150
Comparative Tracking Index 250 V

@Thickness 2.00 mm
250 V

@Thickness 0.0787 in
Solution A; IEC 60112
Hot Wire Ignition, HWI 775 sec

@Thickness 2.00 mm
775 sec

@Thickness 0.0787 in
IEC 60695-2-13
775 sec

@Thickness 3.00 mm
775 sec

@Thickness 0.118 in
IEC 60695-2-13
800 sec

@Thickness 1.00 mm
800 sec

@Thickness 0.0394 in
IEC 60695-2-13