Styron CALIBREâ„¢ 303V-10 Polycarbonate Resin

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer Styron
Trade Name CALIBRE™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Styron CALIBREâ„¢ 303V-10 Polycarbonate Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Overview: CALIBREâ„¢ 300V-10 Polycarbonate resins offer exceptional impact resistance, heat distortion resistance, optical clarity and meets UL94 V-2 rating. CALIBRE 300V series products are available in 3 additive packages: CALIBRE 301V: Mold release. CALIBRE 302V: UV stabilizer. CALIBRE 303V: Mold release and UV stabilizer.Govt. and Industry Standards: CSA (Canadian Standards Association)Underwriters Laboratory Inc. (UL) Applications:Electronic components LightingStorage Media HousingsInformation provided by Styron
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ISO 1183/B; ASTM D792
Water Absorption 0.25 %

@Temperature 23.0 °C
0.25 %

@Temperature 73.4 °F
Equilibrium, 50% RH; ISO 62; ASTM D570
0.15 %

@Temperature 23.0 °C,
Time 86400 sec
0.15 %

@Temperature 73.4 °F,
Time 24.0 hour
ISO 62; ASTM D570
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
ISO 294-4; ASTM D955
Melt Flow 10 g/10 min
10 g/10 min
ASTM D1238
10 g/10 min

@Load 1.20 kg,
Temperature 300 °C
10 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 71.0 MPa
10300 psi
ISO 527-2/50; ASTM D638
Tensile Strength, Yield 60.0 MPa
8700 psi
ISO 527-2/50; ASTM D638
Elongation at Break 150 %
150 %
ISO 527-2/50; ASTM D638
Elongation at Yield 6.0 %
6.0 %
ISO 527-2/50; ASTM D638
Tensile Modulus 2.30 GPa
334 ksi
ISO 527-2/50
2.41 GPa
350 ksi
ASTM D638
Flexural Strength 96.5 MPa
14000 psi
ASTM D790
97.0 MPa
14100 psi
2.0 mm/min; ISO 178
Flexural Modulus 2.40 GPa
348 ksi
2.0 mm/min; ISO 178
2.41 GPa
350 ksi
ASTM D790
Izod Impact, Notched 9.10 J/cm

@Temperature 23.0 °C
17.0 ft-lb/in

@Temperature 73.4 °F
ISO 180/4A
Izod Impact, Unnotched (ISO) NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ASTM D256; ISO 180
Charpy Impact, Notched 3.50 J/cm²

@Temperature 23.0 °C
16.7 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Dart Drop, Total Energy 87.0 J
64.2 ft-lb
ASTM D3763
Abrasion 45
45
[%] Taber; ASTM D1044
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 68.0 µm/m-°C
37.8 µin/in-°F
ASTM D696
Hot Ball Pressure Test 125 °C
257 °F
IEC 60335-1
Deflection Temperature at 0.46 MPa (66 psi) 141 °C
286 °F
Annealed; ISO 75-2/B; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 122 °C
252 °F
Unannealed; ISO 75-2/A
125 °C
257 °F
Unannealed; ASTM D648
138 °C
280 °F
Annealed; ASTM D648
143 °C
289 °F
Annealed; ISO 75-2/A
Vicat Softening Point 146 °C
295 °F
ISO 306/B50; ASTM D1525
Flammability, UL94 V-2

@Thickness 1.60 mm
V-2

@Thickness 0.0630 in
V-2

@Thickness 3.20 mm
V-2

@Thickness 0.126 in
Oxygen Index 26 %
26 %
ISO 4289-2
Optical Properties Metric English Comments
Refractive Index 1.586
1.586
ASTM D542; ISO 489
Haze 1.0 %
1.0 %
ASTM D1003
Transmission, Visible 89 %
89 %
ASTM D1003
Electrical Properties Metric English Comments
Volume Resistivity 2.00e+17 ohm-cm
2.00e+17 ohm-cm
ASTM D257
Dielectric Constant 3.0

@Frequency 60.0 Hz
3.0

@Frequency 60.0 Hz
ASTM D150
3.0

@Frequency 1.00e+6 Hz
3.0

@Frequency 1.00e+6 Hz
ASTM D150
Dielectric Strength 17.0 kV/mm
432 kV/in
ASTM D149
17.0 kV/mm
432 kV/in
IEC 60243-1
Dissipation Factor 0.0010
0.0010
ASTM D150
Comparative Tracking Index 250 V

@Thickness 2.00 mm
250 V

@Thickness 0.0787 in
Solution A; IEC 60112