Styron CALIBREâ„¢ 303V-15 Polycarbonate Resin

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer Styron
Trade Name CALIBRE™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Styron CALIBREâ„¢ 303V-15 Polycarbonate Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Overview: CALIBREâ„¢ 300V-15 Series Polycarbonate resins offer exceptional impact resistance, heat distortion resistance, optical clarity and meets UL94 V-2 rating. CALIBRE 300V series products are available in 2 additive packages: CALIBRE 302V: UV stabilizer. CALIBRE 303V: Mold release and UV stabilizer.Govt. and Industry Standards: CSA (Canadian Standards Association)Underwriters Laboratory Inc. (UL) Applications:Electronic components LightingStorage Media HousingsInformation provided by Styron
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ISO 1183/B
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
ISO 294-4
Melt Flow 15 g/10 min

@Load 1.20 kg,
Temperature 300 °C
15 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 71.0 MPa
10300 psi
ISO 527-2/50
Tensile Strength, Yield 60.0 MPa
8700 psi
ISO 527-2/50
Elongation at Break 150 %
150 %
ISO 527-2/50
Elongation at Yield 6.0 %
6.0 %
ISO 527-2/50
Tensile Modulus 2.30 GPa
334 ksi
ISO 527-2/50
Flexural Strength 97.0 MPa
14100 psi
2.0 mm/min; ISO 178
Flexural Modulus 2.40 GPa
348 ksi
2.0 mm/min; ISO 178
Izod Impact, Notched 8.50 J/cm

@Temperature 23.0 °C
15.9 ft-lb/in

@Temperature 73.4 °F
ISO 180/4A
Charpy Impact, Notched 2.50 J/cm²

@Temperature 23.0 °C
11.9 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Hot Ball Pressure Test 125 °C
257 °F
IEC 60335-1
Deflection Temperature at 0.46 MPa (66 psi) 140 °C
284 °F
Annealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 121 °C
250 °F
Unannealed; ISO 75-2/A
137 °C
279 °F
Annealed; ISO 75-2/A
Vicat Softening Point 145 °C
293 °F
ISO 306/B50
Flammability, UL94 V-2

@Thickness 1.60 mm
V-2

@Thickness 0.0630 in
V-2

@Thickness 3.20 mm
V-2

@Thickness 0.126 in
Electrical Properties Metric English Comments
Comparative Tracking Index 250 V

@Thickness 2.00 mm
250 V

@Thickness 0.0787 in
Solution A; IEC 60112
Users viewing this material also viewed the following: