Performance Features: General purpose, high adhesion to paper and olefin substrates, low stiffness, water resistanceApplications: General Purpose AdhesiveLatin America/South AmericaInformation provided by Styron
Physical Properties Metric English Comments
Solids Content 46 %
46 %
pH 9.0
9.0
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -22.0 °C
-7.60 °F