Styron DL 242NA Functionalized SB

Category Polymer , Thermoplastic , Styrene-Butadiene
Manufacturer Styron
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Styron DL 242NA Functionalized SB.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Performance Features: Glass fiber sizing, reactive with external cross-linkersApplications: Fiber Binding, Glass Fiber Binding, Nonwovens and Thermo MoldableLatin America/South AmericaInformation provided by Styron
Physical Properties Metric English Comments
Solids Content 49 %
49 %
pH 6.5
6.5
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 41.0 °C
106 °F