Styron DL 396 Carboxylated SB

Category Polymer , Thermoplastic , Styrene-Butadiene
Manufacturer Styron
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Styron DL 396 Carboxylated SB.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Performance Features: Heat sealable, low odor, high water resistance, casein compatibilityApplications: Foil Lamination (FSK), Heat Sealable and Lamination (Metalized Paper)EuropeInformation provided by Styron
Physical Properties Metric English Comments
Solids Content 50.5 %
50.5 %
pH 5.7
5.7
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 10.0 °C
50.0 °F