Styron DL264PA Carboxylated SB

Category Polymer , Thermoplastic , Styrene-Butadiene
Manufacturer Styron
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Styron DL264PA Carboxylated SB.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Performance Features: High adhesion to paper and foil substratesApplications: Foil Laminated (FSK) and Laminated (Metalized Paper) Asia PacificInformation provided by Styron
Physical Properties Metric English Comments
Solids Content 52 %
52 %
pH 6.0
6.0
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 15.5 °C
59.9 °F