Material Notes:
Overview: MAGNUM™ ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ABS resins are available in a wide range of melt flow rates, impact strength and heat resistance for both high and low gloss applications manufactured by injection molding, sheet or profile extrusion and thermoforming processes. Automotive MAGNUM ABS resins offer a wide range of gloss, viscosity, impact strength and heat properties for use in numerous automotive applications. Melt flow rates from 1 to 12 g/10 min, impact strengths from 2.4 to 11 ft-lb/in and heat distortion temperatures from 117 to 194°F are available. Available primarily as natural plus concentrates, MAGNUM ABS resins are used in a wide variety of automotive applications including structural instrument panels, consoles, pillars, and exterior trim parts requiring painting and plating. MAGNUM 347 HP ABS resin is a higher flow version of 342 EZ having slightly lower impact strength. The melt flow rate of approximately 12 g/10 min is often suitable for parts with long flow lines and minimal impact requirements.Information provided by Styron
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ASTM D792
Maximum Moisture Content 0.10
0.10
Linear Mold Shrinkage, Flow 0.0040 - 0.0070 cm/cm
0.0040 - 0.0070 in/in
ASTM D955
Melt Flow 12 g/10 min

@Load 3.80 kg,
Temperature 230 °C
12 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 41.4 MPa
6000 psi
Type I, 51 mm/min; ASTM D638
Elongation at Break 30 %
30 %
Type I, 51 mm/min; ASTM D638
Elongation at Yield 2.5 %
2.5 %
Type I, 51 mm/min; ASTM D638
Tensile Modulus 2.07 GPa
300 ksi
Type I, 51 mm/min; ASTM D638
Flexural Strength 65.5 MPa
9500 psi
Type I, 1.3 mm/min; ASTM D790
Flexural Modulus 2.17 GPa
315 ksi
Type I, 1.3 mm/min; ASTM D790
Izod Impact, Notched 1.30 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
2.44 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
0.25 mm Notch Depth; ASTM D256
Dart Drop, Total Energy 73.9 J

@Thickness 3.20 mm,
Temperature 23.0 °C
54.5 ft-lb

@Thickness 0.126 in,
Temperature 73.4 °F
3.39 m/sec, Total Energy; ASTM D3763
85.0 J

@Thickness 3.20 mm,
Temperature 23.0 °C
62.7 ft-lb

@Thickness 0.126 in,
Temperature 73.4 °F
3.39 m/sec, Peak Energy; ASTM D3763
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 85.0 °C

@Thickness 3.20 mm
185 °F

@Thickness 0.126 in
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 73.9 °C

@Thickness 3.20 mm
165 °F

@Thickness 0.126 in
Unannealed; ASTM D648
Vicat Softening Point 102 °C
216 °F
ASTM D1525
Processing Properties Metric English Comments
Melt Temperature 216 - 232 °C
421 - 450 °F
Mold Temperature 26.7 - 48.9 °C
80.1 - 120 °F
Drying Temperature 82.2 - 85.0 °C
180 - 185 °F
Dry Time 2.00 - 4.00 hour
2.00 - 4.00 hour
Back Pressure 0.345 - 3.45 MPa
50.0 - 500 psi
Descriptive Properties Value Comments
Clamp Tonnage 2.8-4.1 kN/cm2
Screw Compression Ratio 1.5:1 to 3.5:1
Screw L/D Ratio 0.834027777777778