Material Notes:
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ABS resin are available in a wide range of melt flow rates, impact strength and heat resistance for both high and low gloss applications manufactured by injection molding, sheet or profile extrusion and thermoforming.The 2600 series of MAGNUM ABS resins are designated for use in healthcare applications. Both high and low gloss resins are available which have passed the USP XXIII Class IV medical testing. Other non-USP classified testing is also done on the MAGNUM 2600 series of ABS resins to evaluate the biocompatibility of the resins.MAGNUM 2630 ABS resin offers the highest impact strength in the healthcare product line. With an Izod strength of 400 J/m, MAGNUM 2630 is applicable for applications requiring this type of impact resistance in a high gloss resin.Data provided by Dow Chemical.This product line was spun off from Dow Chemical to Styron in 2010.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ASTM Data
Linear Mold Shrinkage 0.0055 cm/cm
0.0055 in/in
Melt Flow 2.5 g/10 min

@Load 3.80 kg,
Temperature 230 °C
2.5 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM Data
Mechanical Properties Metric English Comments
Hardness, Rockwell R 101
101
Tensile Strength, Ultimate 31.0 MPa
4500 psi
ASTM Data
Tensile Strength, Yield 37.2 MPa
5400 psi
ASTM Data
Elongation at Break 55 %
55 %
ASTM Data
Elongation at Yield 2.4 %
2.4 %
ISO Data
Tensile Modulus 1.93 GPa
280 ksi
ASTM Data
Izod Impact, Notched 4.00 J/cm
7.49 ft-lb/in
ASTM Data
Charpy Impact Unnotched NB
NB
ISO Data
NB
NB
ISO Data, Low Temp
Charpy Impact, Notched 1.50 J/cm²
7.14 ft-lb/in²
ISO Data, Low Temp
3.20 J/cm²
15.2 ft-lb/in²
ISO Data
Impact Test 50.0 J

@Temperature 23.0 °C
36.9 ft-lb

@Temperature 73.4 °F
Instrumented Dart Total Energy
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 100 µm/m-°C

@Temperature 20.0 °C
55.6 µin/in-°F

@Temperature 68.0 °F
ISO data
Deflection Temperature at 0.46 MPa (66 psi) 93.0 °C
199 °F
Unannealed; ASTM Data
Deflection Temperature at 1.8 MPa (264 psi) 78.0 °C
172 °F
Unannealed; 100°C (212°F) annealed; ASTM Data
Vicat Softening Point 107 °C
225 °F
Optical Properties Metric English Comments
Gloss 95 %
95 %
Gardner Gloss, 60°