Material Notes:
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ABS resin are available in a wide range of melt flow rates, impact strength and heat resistance for both high and low gloss applications manufactured by injection molding, sheet or profile extrusion and thermoforming.The Automotive grades of MAGNUM ABS resins offer a wide range of gloss, viscosity, impact strength and heat properties for use in numerous automotive applications. Melt flow rates from 1 to 12 g/10 min, impact strengths from 130 to 590 J/m and heat distortion temperatures from 77.C to 90.C are available. Available primarily as natural plus concentrates, MAGNUM ABS resins are used in a wide variety of automotive applications including structural instrument panels, consoles, pillars and exterior trim parts requiring painting and plating.MAGNUM 347EZ ABS resin is a higher flow version of 342EZ having slightly lower impact strength. The melt flow rate of about 12 g/10 min is often suitable for parts with long flow lines and less stringent impact requirements.Data provided by Dow Chemical.This product line was spun off from Dow Chemical to Styron in 2010.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ASTM Data
Linear Mold Shrinkage 0.0055 cm/cm
0.0055 in/in
Melt Flow 15 g/10 min

@Load 3.80 kg,
Temperature 230 °C
15 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM Data
Mechanical Properties Metric English Comments
Tensile Strength, Yield 37.9 MPa
5500 psi
ASTM Data
Elongation at Break 110 %
110 %
ASTM Data
Tensile Modulus 2.07 GPa
300 ksi
ASTM Data
Izod Impact, Notched 1.33 J/cm
2.49 ft-lb/in
ASTM Data
Impact Test 16.0 J

@Temperature -30.0 °C
11.8 ft-lb

@Temperature -22.0 °F
Instrumented Dart Total Energy
35.0 J

@Temperature 23.0 °C
25.8 ft-lb

@Temperature 73.4 °F
Instrumented Dart Total Energy
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 72.0 µm/m-°C

@Temperature 20.0 °C
40.0 µin/in-°F

@Temperature 68.0 °F
ASTM data
Deflection Temperature at 0.46 MPa (66 psi) 68.0 °C
154 °F
Unannealed; ASTM Data
Deflection Temperature at 1.8 MPa (264 psi) 77.0 °C
171 °F
Unannealed; ASTM Data
Vicat Softening Point 103 °C
217 °F