Styron PULSE™ EXT 100 PC/ABS Engineering Resin

Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC)
Manufacturer Styron
Trade Name PULSE™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Styron PULSE™ EXT 100 PC/ABS Engineering Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Overview: PULSE EXT 100 engineering resin has been designed to provide excellent processability, high heat resistance, and high impact strength at both room and low temperatures. PULSE EXT 100 engineering resin has been used in automotive exterior trim applications.Information provided by Styron
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ASTM D792
Melt Density 1.02 g/cc
0.0368 lb/in³
Linear Mold Shrinkage, Flow 0.0060 cm/cm
0.0060 in/in
ASTM D955
Melt Flow 1.3 g/10 min

@Load 3.80 kg,
Temperature 230 °C
1.3 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 51.7 MPa
7500 psi
Type I, 51 mm/min; ASTM D638
Elongation at Break 80 %
80 %
Type I, 51 mm/min; ASTM D638
Flexural Yield Strength 82.7 MPa
12000 psi
ASTM D790
Flexural Modulus 2.24 GPa
325 ksi
ASTM D790
Izod Impact, Notched 4.80 J/cm

@Thickness 3.20 mm,
Temperature -29.0 °C
8.99 ft-lb/in

@Thickness 0.126 in,
Temperature -20.2 °F
0.25 mm Notch Depth, Injection Molded; ASTM D256
6.40 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
12.0 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
0.25 mm Notch Depth, Injection Molded; ASTM D256
Dart Drop, Total Energy 54.2 J

@Thickness 3.20 mm,
Temperature 23.0 °C
40.0 ft-lb

@Thickness 0.126 in,
Temperature 73.4 °F
3.39 m/sec; ASTM D3763
59.9 J

@Thickness 3.20 mm,
Temperature -29.0 °C
44.2 ft-lb

@Thickness 0.126 in,
Temperature -20.2 °F
3.39 m/sec; ASTM D3763
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 72.0 µm/m-°C

@Temperature -40.0 - 82.0 °C
40.0 µin/in-°F

@Temperature -40.0 - 180 °F
ASTM D696
Specific Heat Capacity 1.98 J/g-°C
0.473 BTU/lb-°F
Melt; ASTM C351
Thermal Conductivity 0.260 W/m-K
1.80 BTU-in/hr-ft²-°F
Melt; ASTM C177
Deflection Temperature at 0.46 MPa (66 psi) 124 °C
255 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 107 °C
225 °F
Unannealed; ASTM D648
Descriptive Properties Value Comments
Ejection Temperature 138°C
No Flow Temperature 160°C