Styron Pulse® 710 ABS + Polycarbonate

Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC)
Manufacturer Styron
Trade Name Pulse®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Styron Pulse® 710 ABS + Polycarbonate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PULSE® 710 Engineering resin has been designed to provide excellent processability, high heat resistance, and high impact strength at both room and low temperatures. PULSE 710 Engineering resin has been used in automotive interior trim applications.Data provided by Dow Chemical.This product line was spun off from Dow Chemical to Styron in 2010.
Physical Properties Metric English Comments
Density 1.12 g/cc
0.0405 lb/in³
ASTM Data
Melt Density 1.01 g/cc
0.0365 lb/in³
Melt density
Water Absorption 0.15 %
0.15 %
Moisture Absorption at Equilibrium 0.32 %
0.32 %
Humidity Absorption
Linear Mold Shrinkage 0.0070 cm/cm
0.0070 in/in
Melt Flow 4.0 g/10 min

@Load 3.80 kg,
Temperature 230 °C
4.0 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM Data
Mechanical Properties Metric English Comments
Hardness, Rockwell R 110
110
Tensile Strength, Ultimate 44.8 MPa
6500 psi
ASTM Data
Tensile Strength, Yield 51.0 MPa
7400 psi
ASTM Data
Elongation at Break 125 %
125 %
ASTM Data
Elongation at Yield 3.7 %
3.7 %
ISO Data
Tensile Modulus 2.00 GPa
290 ksi
ISO Data.
Izod Impact, Notched 6.41 J/cm
12.0 ft-lb/in
ASTM Data
5.34 J/cm

@Temperature -50.0 °C
10.0 ft-lb/in

@Temperature -58.0 °F
ASTM Data
Charpy Impact Unnotched NB
NB
ISO Data, Low Temp
NB
NB
ISO Data
Charpy Impact, Notched 6.20 J/cm²
29.5 ft-lb/in²
ISO Data, Low Temp
7.90 J/cm²
37.6 ft-lb/in²
ISO Data
Impact Test 56.5 J

@Temperature 23.0 °C
41.7 ft-lb

@Temperature 73.4 °F
Instrumented Dart Total Energy
62.2 J

@Temperature -30.0 °C
45.9 ft-lb

@Temperature -22.0 °F
Instrumented Dart Total Energy
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 73.8 µm/m-°C

@Temperature 20.0 °C
41.0 µin/in-°F

@Temperature 68.0 °F
ASTM data
Specific Heat Capacity 2.54 J/g-°C
0.607 BTU/lb-°F
Thermal Conductivity 0.233 W/m-K
1.62 BTU-in/hr-ft²-°F
Deflection Temperature at 1.8 MPa (264 psi) 98.9 °C
210 °F
Unannealed; 113°C (235°F) annealed; ASTM Data