Styron XU 31591.00 SB Latex

Category Polymer , Thermoplastic , Styrene-Butadiene
Manufacturer Styron
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Styron XU 31591.00 SB Latex.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Performance Features: Good water resistance and elasticityApplications: Waterproofing MembranesNorth AmericaInformation provided by Styron
Physical Properties Metric English Comments
Solids Content 50 %
50 %
pH 7.5
7.5
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -20.0 °C
-4.00 °F