Styron XZ 94462.04 Carboxylated SB

Category Polymer , Thermoplastic , Styrene-Butadiene
Manufacturer Styron
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Styron XZ 94462.04 Carboxylated SB.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Performance Features: Very soft tacky filmApplications: Fiber Binding and NonwovensEuropeInformation provided by Styron
Physical Properties Metric English Comments
Solids Content 47 %
47 %
pH 8.0
8.0
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -45.0 °C
-49.0 °F