Styron XZ 94714.01 Carboxylated SB

Category Polymer , Thermoplastic , Styrene-Butadiene
Manufacturer Styron
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Styron XZ 94714.01 Carboxylated SB.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Performance Features: Anti-corrosion primerApplications: Fiber Binding, Glass Fiber Binding, Nonwovens and Thermo MoldableEuropeInformation provided by Styron
Physical Properties Metric English Comments
Solids Content 49 %
49 %
pH 7.0
7.0
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 18.0 °C
64.4 °F