Styron XZ 97211.00 Carboxylated SB

Category Polymer , Thermoplastic , Styrene-Butadiene
Manufacturer Styron
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Styron XZ 97211.00 Carboxylated SB.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Performance Features: Optimized for melamine and reactive resin based systemsApplications: Nonwovens and Wipes and TissueEuropeInformation provided by Styron
Physical Properties Metric English Comments
Solids Content 49 %
49 %
pH 8.5
8.5
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 12.0 °C
53.6 °F