Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Sumitomo Bakelite Durez® 32245 Phenolic, Compression Grade

Category Polymer , Thermoset , Phenolic
Manufacturer Sumitomo Bakelite High Peformance Plastics
Trade Name Durez®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sumitomo Bakelite Durez® 32245 Phenolic, Compression Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Durez 32245 Black Phenolic is a two-stage glass fiber and mineral filled special purpose molding compound. It is especially designed for applications requiring high strength and dimensional stability with excellent heat resistance. Typical applications include heavy duty switch gear, connectors, and commutators.Information provided by Sumitomo Bak North America, Inc.
Physical Properties Metric English Comments
Bulk Density 0.850 g/cc
0.0307 lb/in³
ASTM D1895
Density 1.80 g/cc
0.0650 lb/in³
ASTM D792
Water Absorption 0.050 %
0.050 %
ASTM D570
Linear Mold Shrinkage 0.0025 cm/cm
0.0025 in/in
ASTM D6289
Mechanical Properties Metric English Comments
Tensile Strength at Break 69.0 MPa
10000 psi
ASTM D638
Tensile Modulus 17.2 GPa
2490 ksi
ASTM D638
Flexural Strength 103 MPa
14900 psi
ASTM D790
Compressive Strength 241 MPa
35000 psi
ASTM D695
Izod Impact, Notched 0.374 J/cm
0.701 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 180 °C
356 °F
UL Temperature Index; at 3.0 mm
Deflection Temperature at 1.8 MPa (264 psi) 204 °C
399 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
V-0

@Thickness 3.00 mm
V-0

@Thickness 0.118 in
V-0

@Thickness 6.00 mm
V-0

@Thickness 0.236 in
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+12 ohm-cm
1.00e+12 ohm-cm
ASTM D257
Dielectric Constant 4.9

@Frequency 1.00e+6 Hz
4.9

@Frequency 1.00e+6 Hz
ASTM D150
Dielectric Strength 13.8 kV/mm
351 kV/in
step-by-step; ASTM D149
17.7 kV/mm
450 kV/in
short time; ASTM D149
Dissipation Factor 0.020

@Frequency 1.00e+6 Hz
0.020

@Frequency 1.00e+6 Hz
ASTM D150
Descriptive Properties Value Comments
Color Black
Molding Method Compression
Users viewing this material also viewed the following: