Material Notes:
Hiprolon® 70 NN is medium viscosity polyamide 6.10 containing a bio-renewable resource. Features: low density, low water absorption, high dimension stability, high notched impact resistance, good chemical resistance. It is widely used as a resin for further compounding, general injection molding and extrusion.Information provided by Suzhou Hipro Polymers Co. Ltd
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
ISO 1183
Water Absorption 1.4 %
1.4 %
ISO 62
Mechanical Properties Metric English Comments
Tensile Strength, Yield 62.0 MPa
8990 psi
ISO 527-1/-2
Elongation at Break >= 50 %
>= 50 %
ISO 527-2/1A
Tensile Modulus 2.30 GPa
334 ksi
ISO 527-1/-2
Flexural Modulus 1.90 GPa
276 ksi
ISO 178
Thermal Properties Metric English Comments
Melting Point 222 °C
432 °F
ISO 11357-3
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C
140 °F
ISO 75-1/2