Sylvin Technologies 9999-85 Natural PVC Molding Compound

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Molded
Manufacturer Sylvin Technologies
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sylvin Technologies 9999-85 Natural PVC Molding Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Sylvin Technologies Inc.
Physical Properties Metric English Comments
Specific Gravity 1.58 g/cc
1.58 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 85
85
10 seconds
Tensile Strength, Ultimate 12.93 MPa
1875 psi
Elongation at Break 310 %
310 %
Tear Strength Test 360
360
Processing Properties Metric English Comments
Melt Temperature 168 - 179 °C
335 - 355 °F