Category | Carbon , Carbon Black , Other Engineering Material , Additive/Filler for Polymer |
Manufacturer | TIMCAL |
Trade Name | C-THERM™ |
Port | Ningbo port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Download PDF | TIMCAL C-THERM™ 001 Graphite Additive for Thermally Conductive Polymers.pdf ![]() |
Price | EMAIL US sales@lookpolymers.com |
Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.150 g/cc | 0.00542 lb/in³ | Scott |
Ash | <= 0.3 % | <= 0.3 % |
Descriptive Properties | Value | Comments |
---|---|---|
Aspect | Form | Soft Granules |