Material Notes:
TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all production and processing stages, strict final inspection, and clearly defined development processes.TIMREX Primary Synthetic Graphite shows unique properties thanks to the combination of a consistent purity, perfect crystalline structure and well defined texture.Tribological and mechanical properties:High toughnessGood lubrication propertiesAdvantages and applications: Low friction coefficientLow wear of the counterpart and low self-wearGood transfer-film formationMedium electrical conductivityMedium density of brushes and partsSuitable for pitch-bonded and resin-bonded brushesInformation provided by TIMCAL
Physical Properties Metric English Comments
Bulk Density 0.330 g/cc
0.0119 lb/in³
Scott
Particle Size 43 µm
43 µm
springback 20.5%, pressure at 0.477 t/cc
45 - 76 µm
45 - 76 µm
d90, Guaranteed
61 µm
61 µm
d90, Typical
70 µm
70 µm
at a density of 2.20 g/cc
75 µm
75 µm
springback 23%, pressure at 0.477 t/cc
145 µm
145 µm
springback 24%, pressure at 0.477 t/cc
625 µm
625 µm
at a density of 2.10 g/cc
1500 µm
1500 µm
at a density of 2.02 g/cc
Deformation 1.1 %
1.1 %
elastic
2.6 %
2.6 %
plastic
3.7 %
3.7 %
plastic + elastic
Ash 0.030 %
0.030 %
Typical
<= 0.10 %
<= 0.10 %
Guaranteed
Thermal Properties Metric English Comments
Thermal Conductivity 130 W/m-K
902 BTU-in/hr-ft²-°F
Electrical Properties Metric English Comments
Electrical Resistivity 2.25 ohm-cm
2.25 ohm-cm
particle size 40 um, pressure at 2.5 t/cc
2.50 ohm-cm
2.50 ohm-cm
particle size 70 um, pressure at 2.5 t/cc
Processing Properties Metric English Comments
Moisture Content 0.020 %
0.020 %
Typical
<= 0.50 %
<= 0.50 %
Guaranteed
Descriptive Properties Value Comments
Crystallite Height, Lc >100 nm
DBP absorption 70 g/100g
(Dibutylphthalate)