Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

TIMET TIMETAL® 367 (Ti-6Al-7Nb) Titanium Alloy

Category Metal , Nonferrous Metal , Titanium Alloy , Alpha/Beta Titanium Alloy
Manufacturer TIMET
Trade Name TIMETAL®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TIMET TIMETAL® 367 (Ti-6Al-7Nb) Titanium Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Medium-Strength Surgical Implant AlloyFeatures: TIMETAL 367 is a dedicated, medium strength, titanium alloy for surgical implants. The alloy was developed specifically for the manufacture of femoral component items for hip prostheses. Its metallurgy is closely analogous to that of TIMETAL 6-4 but biocompatibility is improved with the replacement of vanadium by niobium.Typical heat treatment for this alloy: Anneal at 700°C for 1 hour, air cool. Data provided by TIMET.
Physical Properties Metric English Comments
Density 4.52 g/cc
0.163 lb/in³
Typical
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate >= 900 MPa
>= 131000 psi
Tensile Strength, Yield >= 800 MPa

@Strain 0.200 %
>= 116000 psi

@Strain 0.200 %
Elongation at Break >= 10 %
>= 10 %
Reduction of Area 35 %
35 %
Modulus of Elasticity 105 - 120 GPa
15200 - 17400 ksi
Typical
Fatigue Strength 500 MPa

@# of Cycles 1.00e+7
72500 psi

@# of Cycles 1.00e+7
rotating bend
Thermal Properties Metric English Comments
Beta Transus 1015 °C
1859 °F
Component Elements Properties Metric English Comments
Aluminum, Al 5.5 - 6.5 %
5.5 - 6.5 %
Carbon, C <= 0.080 %
<= 0.080 %
Hydrogen, H <= 0.0090 %
<= 0.0090 %
Iron, Fe <= 0.25 %
<= 0.25 %
Niobium, Nb (Columbium, Cb) 6.5 - 7.5 %
6.5 - 7.5 %
Nitrogen, N <= 0.050 %
<= 0.050 %
Oxygen, O <= 0.20 %
<= 0.20 %
Tantalum, Ta <= 0.50 %
<= 0.50 %
Titanium, Ti 84.5 - 88 %
84.5 - 88 %
Calculated as remainder
Users viewing this material also viewed the following: