Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, 350ºF Cure Temperature

Category Polymer , Thermoset , Polyester, TS , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, 350ºF Cure Temperature.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is carried out by the use of various peroxides including dicumyl peroxide (DCP) or 2,5-dimethyl-2,5-bis (t-butylperoxy) hexane (DBPH).FormulationMillathane 5004100Stearic Acid0.25N330 (HAF) Black20Di-Cup 40C3All information provided by TSE Industries
Mechanical Properties Metric English Comments
Hardness, Shore A 68
68
Tensile Strength, Yield 29.0 MPa
4200 psi
Elongation at Yield 660 %
660 %
100% Modulus 0.00269 GPa
0.390 ksi
200% Modulus 0.00579 GPa
0.840 ksi
300% Modulus 0.0103 GPa
1.49 ksi
Tear Strength 87.6 kN/m
500 pli
ASTM Die C
Processing Properties Metric English Comments
Cure Time 3.00 min

@Temperature 177 °C
0.0500 hour

@Temperature 350 °F
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved