TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, Hardness 70A

Category Polymer , Thermoset , Polyester, TS , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer TSE Industries, Inc
Trade Name Millathane®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, Hardness 70A.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is carried out by the use of various peroxides including dicumyl peroxide (DCP) or 2,5-dimethyl-2,5-bis (t-butylperoxy) hexane (DBPH).FormulationMillathane 5004100Stearic Acid0.25Hi-Sil 23320Di-Cup 40C4All information provided by TSE Industries
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
Tensile Strength, Yield 25.2 MPa
3660 psi
Elongation at Yield 590 %
590 %
100% Modulus 0.00317 GPa
0.460 ksi
200% Modulus 0.00552 GPa
0.800 ksi
300% Modulus 0.00820 GPa
1.19 ksi
Tear Strength 70.0 kN/m
399 pli
ASTM Die C
Processing Properties Metric English Comments
Cure Time 45.0 min

@Temperature 152 °C
0.750 hour

@Temperature 305 °F