Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, Hardness 82A

Category Polymer , Thermoset , Polyester, TS , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer TSE Industries, Inc
Trade Name Millathane®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, Hardness 82A.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is carried out by the use of various peroxides including dicumyl peroxide (DCP) or 2,5-dimethyl-2,5-bis (t-butylperoxy) hexane (DBPH).FormulationMillathane 5004100Stearic Acid0.25Hi-Sil 23340Di-Cup 40C6All information provided by TSE Industries
Mechanical Properties Metric English Comments
Hardness, Shore A 82
82
Tensile Strength, Yield 20.7 MPa
3000 psi
Elongation at Yield 500 %
500 %
100% Modulus 0.00269 GPa
0.390 ksi
200% Modulus 0.00496 GPa
0.720 ksi
300% Modulus 0.00731 GPa
1.06 ksi
Tear Strength 61.3 kN/m
350 pli
ASTM Die C
Processing Properties Metric English Comments
Cure Time 2.00 min

@Temperature 204 °C
0.0333 hour

@Temperature 400 °F
Copyright © lookpolymers.com All Rights Reserved